Fixing Spatter from Wrong Gas Mix

Wrong gas mixtures create excessive spatter through improper arc characteristics and metal transfer modes. Use appropriate Ar/CO2 ratios for your application - typically 18-25% CO2 for carbon steel.

Recommended

CORGONĀ® 18

Why CORGON 18 reduces spatter: Optimized 18% CO2 content provides excellent balance between penetration and low spatter characteristics.